Dave,
When we evaluate a wave solder flux, one of the tests we perform is to run
SIR and EM coupons facing up, and allow over spray as would be normally seen
at a "heavy" flux application setting. The board then is processed through
preheat and the bottomside exposed to typical wave conditions. SIR and EM
testing is then completed. Of course we also run a set of coupons "down" to
simulate actual exposure to the full effect of fluxing, preheat and wave.
Thanks,
Robert Furrow
Printed Wiring Board Engineer
Supply Chain Networks
Lucent Technologies
978-960-3224 [log in to unmask]
-----Original Message-----
From: David White [mailto:[log in to unmask]]
Sent: Thursday, May 09, 2002 10:33 AM
To: [log in to unmask]
Subject: [TN] Flux on top of PCBs from wave
Technet,
Is anyone concerned about the over spray of flux on the top of PCB
assemblies. We use generic pallets in our process, so our PCB's will get
over spray form the spray fluxer, it has recently been brought up as a
concern. We use a no-clean flux (Lonco SLS65). Does anyone else do this
also, and if so do you have the same concerns? The flux can sometimes be
pretty noticeable. I am in the process of getting Ionic testing done, but
would like your experiences.
Dave
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|