TECHNET Archives

June 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Chris Schaefer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Chris Schaefer <[log in to unmask]>
Date:
Tue, 10 Jun 2008 13:44:47 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (29 lines)
Hey all,

Not so long ago there was a company that made a tool that could be adapted 
to most name brand wave solder machines that would allow the user to 
mechanically measure the distance from the nozzle to the conveyor rails. The 
tool was used to make sure that after PM's on the nozzles, they could be sure 
the nozzles were put back into the near exact position they were prior to the 
maintenance. What I want to do is take distance measurements from the 
nozzles to the conveyor rails prior to running a wave rider and use the 
mechanical measurements to better predict the outcome as long as some of 
the other vairiables stay relatively the same. Also, we have a manually 
adjusted solder pot height adjustment system and I want to make sure that 
everytime the pot is set, it is set to the exact position required for optimized 
soldering (as I see it). The machine dial isn't exactly precise and too objective.

Any thoughts. As always, thanks in advance for your help.

Chris

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2