Denis,
I find this as an ongoing challenge that is complicated even further by
ourselves. We all have good information and share our experience and ideas
the best that we can, but........
I find that a lot of the time information on what works and what doesn't is
not recorded properly enough to use as data to substantiate our experiences,
and when it is, it's proprietary information and the property of a company
who won't, or can't, publish it's findings for us to use.
If anybody has a solution to this dilemma, please share.
Allen Maddox
Senior PCB Designer
GAI-Tronics
PO Box 1060
Reading, PA 19607-1060
Voice: 610-796-5854
FAX: 610-777-1870
www.gai-tronics.com
[log in to unmask]
-----Original Message-----
From: Denis Lefebvre [mailto:[log in to unmask]]
Sent: Thursday, May 23, 2002 10:10 AM
Subject: BGA Solderability
<snip>
I am convinced that this will not fare well when they try to solder this
part, yet the engineer insists on doing it this way. What argument can I
make, with supporting data, to persuade him? Simply telling him that I know
it is poor practice isn't cutting it! [Adjusting tie..."I tell ya, we get no
respect!"]
Denis Lefebvre, C.I.D.
Senior PCB Designer
408-542-3832
Finisar Corporation
1308 Moffett Park Drive
Sunnyvale, CA 94086
www.finisar.com <http://www.finisar.com/>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|