TECHNET Archives

August 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"Dorothy M. Lush" <[log in to unmask]>
Date:
Tue, 21 Aug 2001 13:23:56 -0700
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (64 lines)
Who is the maker of the solder paste and what is its name?  We have been
having this problem also where we have not had it before.

Solder balls are formed by: misprinting, too much solder paste, reflow
profile, solder paste slump(ability), crappy solder paste. Take your pick.

Dorothy Lush

> ----------
> From:         Jorge Rodriguez[SMTP:[log in to unmask]]
> Reply To:     TechNet E-Mail Forum.
> Sent:         Tuesday, August 21, 2001 11:57 AM
> To:   [log in to unmask]
> Subject:      Solder Beads (not solder balls)
>
> Fellow technetters,
>
> We are having tons of issues with solder beading, even on boards were we
> didn't have the issue before. We're clueless, we suspect of the solder
> paste
> (63-37 Water Soluble), it looks slumpy amd watery, but we're not sure. I
> know solder beading can be solved by designing the stencils with home-base
> aperture, but what we're seeing here is across the board, not just one
> particular assembly but several. Does anyone have experience dealing with
> an
> issue like this?, could solder beading caused by the oven profile or is it
> more like solder paste related?
>
>
> Any comments would be appreciated.
>
>
> Jorge Rodriguez
> Process Engineer
> Varian Electronics Manufacturing
> E-mail: [log in to unmask]
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2