Hi Victor! You may want to try to get a copy of IPC-GH-850 "Handbook of
Interconnection Contact Finishes" - it has quite a bit of useful
information on finishes and test methodologies. Just a warning - the last
time I recommend someone get a copy of the 850 Handbook the IPC folks had
to do some digging. My copy is dated August 1990 and the Handbook may no
longer be active. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




                      Victor Hernandez
                      <Victor_G_Hernande        To:       [log in to unmask]
                      [log in to unmask]>               cc:
                      Sent by: TechNet          Subject:  [TN] Surface Plating Finish
                      <[log in to unmask]>


                      01/31/2003 09:46
                      AM
                      Please respond to
                      "TechNet E-Mail
                      Forum."; Please
                      respond to
                      Victor_G_Hernandez






Fellow TechNetters:

    Besides Table 4-3  Final Finish, Surface Plating Coating Requirements.
Is there a more comprehensive data metric that also address Insertion
Cycles
per gold plating thickness
on edge-board connectors and areas not to be soldered.   Many suggest
contacting the vendor.  However,
I feel there should be some industry established guideline.

Victor G. Hernandez

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
 -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2