Hello,
Maybe this question is not typical Technet-related, but I think I can find
some solder-expertise on this forum.

By quickly dipping a copperwire of 0.6 mm in a HighMeltingPoint-solderbath
(MP=296 -302°C), we succeed to take up 5 to 15 mgr (±1 mm(superscript: 3))
solder at 5 mm from the end of the wire (our target is 10 mgr). Because
this is a non-equilibrium process the spread is rather high. Nevertheless
we try to improve the reproducability. Important factors which we can
control are:  temperature and  withdrawal speed . Surface tension
(influenced by the flux) and viscosity of the solder must be important too
but difficult to measure and to influence.
I can use any ideas / considerations / information how we can improve the
reproducability.

some other related questions:
-how long works the addition of 100 ppm Phosphor in the solder ?
-which could be the influence of eutectic solder (Pb(subscript: 97.5)Sn
(subscript: 1)Ag(subscript: 1.5)  MP=309°C) versus paste range solder (HMP
Pb(subscript: 93.5)Sn(subscript: 5)Ag(subscript: 1.5)  MP=296-302°C) on the
solidifying and reproducability on the wire?
-we use flux to dip the wire and a scraper to evacuate the dross (lot of
dross!) on the solderbath-surface, we do not know a soldercover(oil) except
the too agressive ammonium-zinc-chlorides; are there alternatives? Bath is
operating at 340°C.
-are there alternative droplet depositioin techniques: what about droplet
deposition by jetting? Feasable?

Thanks in advance,
Jos
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2