TECHNET Archives

April 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Wed, 30 Apr 2008 15:53:32 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (19 lines)
Werner's mentioning of pad design to prevent chip cracking and other
issues discussed recently had me wondering if hot air rework, whether
done by hot-gas rework machines or by using hand-held hot air stations
such as the Hakko, is required for Class 3 hardware. I thought it was,
but cannot find a reference to it in J-STD-001D, -DS, or in the
Handbook. Therefore I am under the assumption that rework of ceramic
chip caps/resistors using standard solder irons is acceptable, even if
not preferred. Is this true?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2