Dear Suganthi,

The process I know of is called "Pin-In-Paste" (also AKA intrusive reflow)
i.e. when the pins of a THT component are paste soldered at the same time
with SMT components by means of reflow process.

Best regards,
Yordan Venev
Manufacturing Manager
********************************************************
CENTILLION LTD.
7-th km Tzarigradsko shosse Blvd.
ATM Center
1784 Sofia, BULGARIA
Tel. :(+359 2) 974 47 51, 965 84 95, 965 58 85
Fax :(+359 2) 974 47 52
mail to: [log in to unmask] <mailto:[log in to unmask]>
www.centillion-bg.com <http://www.centillion-bg.com>


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Selva Suganthi
Sent: Friday, January 06, 2006 1:21 PM
To: [log in to unmask]
Subject: [TN] Paste In-Hole process


Dear All ,

What is called  "Paste In-Hole process" ? , please explain me.

Thanks and Regards
Suganthi
Telephone : 91-44-22540020 Ext 182
eMail : [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
"Progress is the activity of today and the assurance of tomorrow."

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2