Dear Suganthi, The process I know of is called "Pin-In-Paste" (also AKA intrusive reflow) i.e. when the pins of a THT component are paste soldered at the same time with SMT components by means of reflow process. Best regards, Yordan Venev Manufacturing Manager ******************************************************** CENTILLION LTD. 7-th km Tzarigradsko shosse Blvd. ATM Center 1784 Sofia, BULGARIA Tel. :(+359 2) 974 47 51, 965 84 95, 965 58 85 Fax :(+359 2) 974 47 52 mail to: [log in to unmask] <mailto:[log in to unmask]> www.centillion-bg.com <http://www.centillion-bg.com> -----Original Message----- From: TechNet [mailto:[log in to unmask]]On Behalf Of Selva Suganthi Sent: Friday, January 06, 2006 1:21 PM To: [log in to unmask] Subject: [TN] Paste In-Hole process Dear All , What is called "Paste In-Hole process" ? , please explain me. Thanks and Regards Suganthi Telephone : 91-44-22540020 Ext 182 eMail : [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- "Progress is the activity of today and the assurance of tomorrow." --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------