TECHNET Archives

June 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-type:
text/plain; charset="us-ascii"
Sender:
Subject:
From:
Dave Hillman <[log in to unmask]>
Date:
Fri, 14 Jun 2002 16:40:51 -0500
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (69 lines)
Hi Henry! I don't have any specific data on the interaction of
intermetallic growth and solder joint failures other than it is generally
acknowledged that "thick" intermetallics will cause solder joint failures.
I have experience with the reworking of a component between 1-3 times
(using standard/typically semiautomated rework equipment, profiles and
soldering times) and not had any issue with intermetallic phase induced
solder joint failures in high performance product use environment. Take a
look in KleinWassink's book (ISBN 0-901150-14-2), page 95 - there is a
temperature versus time versus intermetallic thickness chart which you can
use to get an idea of how much intermetallic you will create depending on
your soldering process.  Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




Henry Rekers <[log in to unmask]>@ipc.org> on 06/11/2002 04:05:28 PM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
       to Henry Rekers <[log in to unmask]>

Sent by:    TechNet <[log in to unmask]>


To:    [log in to unmask]
cc:

Subject:    [TN] Intermetallic Joint Failure


Does anybody have any data or standards on the amount of times a solder
joint can be re-flowed regarding intermetallic growth and subsequent joint
failure?

We are trying to develop a "rework policy" for a high reliability product.
Our boards are fairly expensive so the trash can is not really an option
unless absolutely necessary.

Thanks.

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2