TECHNET Archives

September 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
KELLY M SCHRIVER <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 10 Sep 1999 11:32:00 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (36 lines)
Daan -

From your description, the condition is starting to sound more like a
"non-wetting" problem than "de-wetting".  Non-wetting being a situation where
the solder never spreads and wets the pad.  Refer to Dave Hillman's earlier
response which discussed the possibility of gold porosity, which could be the
source of your problem.

A simple test to visually confirm the above would be to do a brief solder dip
test on a section of circuit board using an RMA flux similar to that in your
paste.  If the specimen remains gold plated, you have a pretty good indicator
that the condition is non-wetting.  Another test option might be to heat a
specimen with paste on it on a hot plate where it can be observed under
magnification.  If the solder does not spread when it melts, it is an
indication of non-wetting.

Given that you are receiving boards with this same finish from other
suppliers, and processing them successfully, it would seem that your problems
must originate with the new suppliers processes rather than your own.

Regards - Kelly

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2