Tom,
It will depend also on your pad style. We run this way.
0 0
0 0
0 0 ----------->
0 0
0 0
0 0
0 0
0 0
In other word perpindicular to the wave. We are running at close to a zero defect level using a 64X100 mil
pad with traces between and using a no wash system. As geomtries get tighter give up thru hole. THis is
coming from someone who has 12 year experience in thruough hole and has given up the ghost. With SMT run
in opposite and use robber pads or cram your decoupling cap on the as* end of you ic to rob the solder.
i.e
vcc
0 - 0
0 | 0
0 | 0
0 | 0
0 | 0
0 | 0
0 | 0
gnd 0capacitor0
Tom Braswell wrote:
> Netters,
>
> Someone tell me which of these two is correct for wave soldering
>
> 1. Direction thru wave -------------------->
>
> _|__|__|__|__|__
> | |
> | |
> |____________|
> | | | | |
>
> 2. Direction thru Wave ----------------------->
>
> _______
> __| |__
> __| |__
> __| |__
> __| |__
> |_______|
>
> Thanks,
>
> Tom B.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|