Board finish? Let me guess.... Entek?
-----Original Message-----
From: McMonagle, Michael R. [mailto:[log in to unmask]]
Sent: Thursday,June 25,1998 3:30 PM
To: [log in to unmask]
Subject: [TN] Poor Solderability on TSOPs
I am looking for a little enlightenment with an issue that we have been
seeing. We have SMT assemblies with poor solderability on TSOP and
mini-QFP type devices. The solder appears to have incomplete reflow
and/or grainyness to the joints. Everything else on the board such as
chips, j-leads and standard QFPs look good, shiny and well wetted. We
are using fresh aqueous paste (Alpha WS609) and a fairly standard
profile. Is there some inverse relationship between component/lead mass
and thermal absorption that I am missing here? Any inputs would be
greatly appreciated.
Mike McMonagle
Process Engineering Supervisor
K*Tec Electronics
Mike McMonagle
PCA Process Engineering Supervisor
K*Tec Electronics
1111 Gillingham Lane
Sugar Land, TX 77478
281-243-5639 Phone
281-527-1726 Pager
281-243-5539 Fax
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|