Per David's info, IPC-RB-276 has no thickness for fused tin-lead or solder
coating; however; the replacement documents, soon to be issued IPC-6012, has
in Table 3-2 a requirement for unfused tin-lead at a minimum of 8 micron
[0.0003 in] 

Phil Hiinton 
[log in to unmask] 

***************************************************************************