TECHNET Archives

August 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
TechNet Mail Forum<[log in to unmask]>
Subject:
From:
Poh Kong Hui <[log in to unmask]>
Date:
Sat, 30 Aug 1997 00:23:26 +0800
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Poh Kong Hui <[log in to unmask]>
Parts/Attachments:
text/plain (13 lines)
Hi Technetters,

Could anyone give me some advise on the dewetting issue.

One of our component supplier told me that misalignment of the chip
component will cause dewetting.

I haven't heard of such thing before, and couldn't believe so. However, I
would like to hear from others' opinion about this issue, whether this is
of a true statement from my suppiler, stating "Dewetting can be caused by
Misaligment".