Hi Technetters, Could anyone give me some advise on the dewetting issue. One of our component supplier told me that misalignment of the chip component will cause dewetting. I haven't heard of such thing before, and couldn't believe so. However, I would like to hear from others' opinion about this issue, whether this is of a true statement from my suppiler, stating "Dewetting can be caused by Misaligment".