TECHNET Archives

March 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"marvin v. picardal" <[log in to unmask]>
Date:
Thu, 2 Mar 2000 13:00:29 +0200
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Brian Ellis <[log in to unmask]>
Parts/Attachments:
text/plain (57 lines)
Hi, all!

OK, I may have been too categorical in my previous post. It may work for some depending
on the degree of cleanliness they require, the purity of the water, the substrate
material and the surface finish of the material under practical conditions. I maintain
though that the basic premisses of the test are flawed and that universal application
of it may lead to problems and disappointments - or worse.

Caveat utilisator

Brian



"marvin v. picardal" wrote:

> Dear Techneters,
>
> I would like to ask some information as to
> how to detect contamination on metal surface and
> how do I determine what type of contamination that is.
> The said contamination results to poor adhesion
> between the glue and the metal surface.
>
> I do hope you would take time in helping me out with this.
> Thank you in advance.
>
> Marvin
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2