Hi, all! OK, I may have been too categorical in my previous post. It may work for some depending on the degree of cleanliness they require, the purity of the water, the substrate material and the surface finish of the material under practical conditions. I maintain though that the basic premisses of the test are flawed and that universal application of it may lead to problems and disappointments - or worse. Caveat utilisator Brian "marvin v. picardal" wrote: > Dear Techneters, > > I would like to ask some information as to > how to detect contamination on metal surface and > how do I determine what type of contamination that is. > The said contamination results to poor adhesion > between the glue and the metal surface. > > I do hope you would take time in helping me out with this. > Thank you in advance. > > Marvin > > ############################################################## > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c > ############################################################## > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in > the body: > To subscribe: SUBSCRIBE TECHNET <your full name> > To unsubscribe: SIGNOFF TECHNET > ############################################################## > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional > information. > If you need assistance - contact Keach Sasamori at [log in to unmask] or > 847-509-9700 ext.5315 > ############################################################## ############################################################## TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c ############################################################## To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TECHNET <your full name> To unsubscribe: SIGNOFF TECHNET ############################################################## Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information. If you need assistance - contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ##############################################################