TECHNET Archives

August 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
quoted-printable
Sender:
Subject:
From:
Phil Nutting <[log in to unmask]>
Date:
Tue, 14 Aug 2001 08:48:05 -0400
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Parts/Attachments:
text/plain (29 lines)
Ok folks, here is today's question.

I just received a Certificate of Analysis (our first one) for the solder
in our Soltec Waver Solder machine.  All parameters are "within
specification" except the percentage of copper which is at 1.6859. (Tin
is at 61.3% and Lead is at 36.99% and other stuff is at 0.0199%)  We run
63/37 in the wave.  We only solder our own product, none of which goes
into "mission critical" applications.  We normally build our product to
IPC-A-610C, Class 2.

My question is two-fold.  Should I worry about this?  If so, how do I
fix it with 1700 pounds of solder in the solder pot? 

Thanks is advance for sharing your knowledge.

Phil Nutting
Manufacturing Engineer
Kaiser Systems, Inc.

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2