TECHNET Archives

May 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
[log in to unmask], TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 9 May 2008 06:54:08 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (198 lines)
By now you should have realized that I do know words. I am aware of its
meaning and uses/misuses. It was wrong of the IPC-A-600 to use a
colloquial idiom to define something without first determining the
clarity of the meaning; defining it within the document itself or having
it included in IPC-T-50.
Thanks for the additional inputs. There are still a few fine,
distinguished, English Gentlemen that still speak to me. Graham does
too.
Dewey

-----Original Message-----
From: Mike Fenner [mailto:[log in to unmask]] 
Sent: Friday, May 09, 2008 2:58 AM
To: 'TechNet E-Mail Forum'; Whittaker, Dewey (EHCOE)
Subject: RE: [TN] The meaning of "skived"

There is an alternative vernacular meaning to 'Skive' in British
English:
Its a pejorative term for some one not doing something they should. Or
secondarily doing something they shouldn't.
If some one skives off a task it means they are dodging it, making them
a
skiver. So by a small stretch I [mis] understood what it meant fairly
clearly! 
If you were to say the solder is skiving off in conversation, you would
be
saying it is not working or is going to a place or doing something it
shouldn't. 

It could be there was a Brit on the panel and in the discussion he just
said
to himself it's skiving off then, and someone wrote it down thinking it
was
a precise technical term!  Whatever ....it's not a word you would expect
to
see written in a formal document. 

Regards 

Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Thursday, May 08, 2008 8:17 PM
To: [log in to unmask]
Subject: Re: [TN] The meaning of "skived"

I am already pushing for some other changes to IPC-A-600 and this is
IMHO an
incorrect usage of the term. I am not sure of the time frame, but we'll
get
to yours briefly.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Thursday, May 08, 2008 11:46 AM
To: [log in to unmask]
Subject: Re: [TN] The meaning of "skived"

So which ones of you are on the IPC-A-600 committee?
You can consider editing this for the next rev.  Because "skived" is the
word used.

Have a good day, eh? (from another Canadian) 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: May 8, 2008 12:00 PM
To: [log in to unmask]
Subject: Re: [TN] The meaning of "skived"

I am more used to the term skiving as it relates to compliant pins being
pushed into Tin-lead plated-through holes. The skiving results in FOD. 
I think thieving is more in-line with what you are referring to.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Thursday, May 08, 2008 10:34 AM
To: [log in to unmask]
Subject: [TN] The meaning of "skived"

Can anyone define "skived" as in:
IPC-A-600      2.9.3.3   Ball Grid Array (Solder Dam)

"....in order to avoid solder being skived from the attachment joint
into
the via."

Online dictionaries define skive as:	to slice off (leather, rubber,
etc.) in thin layers; shave.

It sort of gives me an idea, but it really isn't very clear.
Thanks in advance.

Genny 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are
intended solely for the addressee(s) and may be legally privileged
and/or confidential. If you are not the intended recipient, please
contact the sender by return and delete the material from any computer.
Any review, retransmission, dissemination, or other use of, or taking of
any action in reliance upon this information by persons or entities
other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery,
and unauthorized alteration. This email has been prepared using
information believed by the author to be reliable and accurate, but
Indium Corporation makes no warranty as to accuracy or completeness.
Indium Corporation does not accept responsibility for changes made to
this email after is was sent. Any opinions or recommendations expressed
herein are solely those of the author. They may be subject to change
without notice.***"

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2