Yes this is all true but you may need to reduce the number of holes in a
mouse bit design for lead free. Also you may see issues with break out on
high tg laminate. The break out section will be rougher. On some materials
much of the resin separates from the glass.
Breakout of boards and the design is never mundane you ask the guys on the
shop floor that at doing it?
Have to say I am "Gobsmacked" by my first trip to Las Vegas, its like
Blackpool/South end in the UK on steroids.
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
Book your place on Bob's "Step by Step Failure Analysis Workshop" 14th May
www.ASKbobwillis.com/faworkshops.pdf
New "Printed Board Inspection & Quality Control" 3 July
www.ASKbobwillis.com/PCBworkshop.pdf
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee parker
Sent: 27 March 2008 17:26
To: [log in to unmask]
Subject: Re: [TN] Breakaway tabs
Eddie
While this may appear to be a very mundane issue it is complicated. For
instance are you using a fixture to hold the board and minimize stress
concentrations. As you suggest, drilling holes along the cut line will help.
Also scoring the tabs along the fracture line will also minimize
delamination. It has been my experience that the breakaway tabs must be
designed to be compatible with the paneling strategy and the board removal
process.
Best regards
Lee
J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: "Eddie Rocha" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, March 27, 2008 12:36 PM
Subject: [TN] Breakaway tabs
> Is there a standard for designing breakaway tabs? Or a standard on how
> much
> mechanical stress during the breaking of tabs should a PCB withstand?
>
> I have a customer that is using tabs .125 wide with no breakaway holes.
> They
> experience slight delamination/fracturing after they break these tabs.
>
> thanks,
> Eddie
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|