TECHNET Archives

August 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Debbie Kenney <[log in to unmask]>
Reply To:
"TechNet E-Mail Forum." <[log in to unmask]>, Debbie Kenney" <[log in to unmask]>
Date:
Wed, 19 Aug 1998 12:04:53 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (41 lines)
Circuit Image Systems carries several excellent gold plating resists
along with technical expertise. You can contact them at (714) 288-4747,
ask for Jerry or Richard.

Good Luck,
Debbie Kenney
M-Flex
[log in to unmask]

> -----Original Message-----
> From: Zecal Engineering [SMTP:[log in to unmask]]
> Sent: Wednesday, August 19, 1998 10:52 AM
> To:   [log in to unmask]
> Subject:      [TN] gold plating resists
>
> We have trouble with dry film lifting during heavy dep gold plating.
> LPI works, but is difficult to strip. Any suggestions?

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2