Circuit Image Systems carries several excellent gold plating resists along with technical expertise. You can contact them at (714) 288-4747, ask for Jerry or Richard. Good Luck, Debbie Kenney M-Flex [log in to unmask] > -----Original Message----- > From: Zecal Engineering [SMTP:[log in to unmask]] > Sent: Wednesday, August 19, 1998 10:52 AM > To: [log in to unmask] > Subject: [TN] gold plating resists > > We have trouble with dry film lifting during heavy dep gold plating. > LPI works, but is difficult to strip. Any suggestions? ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information. For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312 ################################################################