TECHNET Archives

May 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 28 May 2003 14:03:34 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Gary Camac <[log in to unmask]>
Subject:
From:
Gary Camac <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
Organization:
Dickey-john Corp.
MIME-Version:
1.0
Parts/Attachments:
text/plain (26 lines)
Steve,

My man - thanks for sticking with us.  After taking on two kinds cancer over the last few
years I have determined that life has no quarantines, but if I don't take it and myself
too seriously I seem to enjoy it more.

The spec sounds bogus.  I am going to assume you are expecting 0.001" copper in your
holes.  If you start with 0.0005" foil on layer 1 of the laminate,  after hole plate the
etches would be at least 0.0015".   Looking at the stack-up it looks like PWB vendor has
to have a laminate with 1 oz. clad to one side (layer 2 side) and 3/8 oz clad to the other
side (layer 1side).  I guess one of the board guys could say if that is normal, i.e. in
stock, material.

Gary Camac

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2