TECHNET Archives

October 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Tue, 1 Oct 2013 17:14:03 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (134 lines)
Okay here's another picture. I printed a solder sample and sent it
through the oven and this is what it looked like:

http://stevezeva.homestead.com/SolderSample.jpg

You can see all the non-wetting going on. The board  was profiled and it
was fine. We are using a FCT Assembly WS889 SN100C solder paste.

What is even more strange is that the first side of the board looked
okay, but the second side looks like in the photos, like the problem is
confined to one side of the board if that's possible.

The solder sample was only reflowed once, but I printed the paste on the
side that was to be built last. Weird huh?

I know you can't tell anything for sure just from some photos, but it's
the strangest thing I've seen in a while... 

Steve 

-----Original Message-----
From: Steve Gregory 
Sent: Tuesday, October 1, 2013 4:46 PM
To: [log in to unmask]; Steve Gregory
Subject: RE: [TN] HASL question

Here's one picture:

http://stevezeva.homestead.com/NonWetting.jpg

Look at the left pad and the tarnish that you see there, does that look
like tarnished nickel?

This is after the board was washed. I have places all over the board
that looks like this. 

I'll post a picture of what it looks like after I printed a solder
sample with paste and sent it through the reflow over

Steve 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, October 1, 2013 4:16 PM
To: [log in to unmask]
Subject: Re: [TN] HASL question

Ahhhh....it's what I figured. I think that's what happened. I'll have
pictures later.

Steve 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer
Sent: Tuesday, October 1, 2013 4:15 PM
To: [log in to unmask]
Subject: Re: [TN] HASL question

No.  Not unless somebody screwed up.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, October 01, 2013 6:11 PM
To: [log in to unmask]
Subject: Re: [TN] HASL question

Hi all,

It's funny that the HASL topic has come up today, because we just ran a
board today that supposedly was lead-free HASL finished, and man it
looks like crap!

Question; does a PCB get nickel before it gets Lead-free HASL'ed?

Steve 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev.
PhD
Sent: Tuesday, October 1, 2013 2:23 PM
To: [log in to unmask]
Subject: Re: [TN] HASL question

Hello Victor,

 It wouldn't solder in a first palce. 

--
Best regards,

Vladimir Igoshev. PhD
mailto:[log in to unmask]

SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2