Okay here's another picture. I printed a solder sample and sent it through the oven and this is what it looked like: http://stevezeva.homestead.com/SolderSample.jpg You can see all the non-wetting going on. The board was profiled and it was fine. We are using a FCT Assembly WS889 SN100C solder paste. What is even more strange is that the first side of the board looked okay, but the second side looks like in the photos, like the problem is confined to one side of the board if that's possible. The solder sample was only reflowed once, but I printed the paste on the side that was to be built last. Weird huh? I know you can't tell anything for sure just from some photos, but it's the strangest thing I've seen in a while... Steve -----Original Message----- From: Steve Gregory Sent: Tuesday, October 1, 2013 4:46 PM To: [log in to unmask]; Steve Gregory Subject: RE: [TN] HASL question Here's one picture: http://stevezeva.homestead.com/NonWetting.jpg Look at the left pad and the tarnish that you see there, does that look like tarnished nickel? This is after the board was washed. I have places all over the board that looks like this. I'll post a picture of what it looks like after I printed a solder sample with paste and sent it through the reflow over Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Tuesday, October 1, 2013 4:16 PM To: [log in to unmask] Subject: Re: [TN] HASL question Ahhhh....it's what I figured. I think that's what happened. I'll have pictures later. Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Wayne Thayer Sent: Tuesday, October 1, 2013 4:15 PM To: [log in to unmask] Subject: Re: [TN] HASL question No. Not unless somebody screwed up. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Tuesday, October 01, 2013 6:11 PM To: [log in to unmask] Subject: Re: [TN] HASL question Hi all, It's funny that the HASL topic has come up today, because we just ran a board today that supposedly was lead-free HASL finished, and man it looks like crap! Question; does a PCB get nickel before it gets Lead-free HASL'ed? Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev. PhD Sent: Tuesday, October 1, 2013 2:23 PM To: [log in to unmask] Subject: Re: [TN] HASL question Hello Victor, It wouldn't solder in a first palce. -- Best regards, Vladimir Igoshev. PhD mailto:[log in to unmask] SENTEC Testing Laboratory Inc. 11 Canadian Road, Unit 7. Scarborough, ON M1R 5G1 Tel: (416) 899-1882 Fax: (905) 882-8812 www.sentec.ca ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________