TECHNET Archives

August 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
TPE Engineering TechNet <[log in to unmask]>
Date:
Mon, 23 Aug 1999 09:52:46 -0700
Content-Type:
text/plain
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, TPE Engineering TechNet <[log in to unmask]>
Parts/Attachments:
text/plain (22 lines)
Steve,
how about using an electric eraser to remove the solder from
the gold tips? You can experiment with different erasers
(more or less abrasive) to see what works best for you. Don't
have to worry about putting in any deep scratches by using
an X-acto blade.
Ron

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2