TECHNET Archives

November 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Eric Dawson <[log in to unmask]>
Date:
Mon, 18 Nov 2002 12:30:49 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Douthit <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii; x-mac-type="54455854"; x-mac-creator="4D4F5353"
From:
David Douthit <[log in to unmask]>
Parts/Attachments:
text/plain (76 lines)
Eric,

 Congratulations! You have proved, once again, that water vapor is much more permeable than liquid water.

Try "soaking"  them in a high humidity condition (>90%) at 40 degrees C for 48 hours then running reflow.

David A. Douthit
Manager
LoCan LLC

Eric Dawson wrote:

> Werner,
> I could use some myself for internal quality training.
> I have recently soaked some BGAs and some quad packs in water for over a
> week before putting them through a reflow profile. I have yet to produce
> visible evidence of pop corning.
> The annoying thing is, a while ago we used some BGAs on a tape where the
> moisture indicator went just a little pink and they pop corned. The visual
> evidence was fat solder deposits and shorts in the middle of the package
> where it bowed downwards. My street cred. with the managers around here has
> taken a beating since I have failed to reproduce the problem.
> Oh well, I'd rather be happy than right.
> Regards
> Eric Dawson
>
> > -----Original Message-----
> > From: Werner Engelmaier [SMTP:[log in to unmask]]
> > Sent: Monday, November 18, 2002 4:02 PM
> > To:   [log in to unmask]
> > Subject:      [TN] Popcorning
> >
> > Hi 'Netters,
> > Could any of share some good pictures of a 'popcorned' component and a
> > component with delaminated die. I would of course give full credit as to
> > source.
> >
> > Thanks,
> > Werner Engelmaier
> >
> > ---------------------------------------------------
> > Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> > To unsubscribe, send a message to [log in to unmask] with following text in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt or (re-start) delivery of Technet send e-mail to
> > [log in to unmask]: SET Technet NOMAIL or (MAIL)
> > To receive ONE mailing per day of all the posts: send e-mail to
> > [log in to unmask]: SET Technet Digest
> > Search the archives of previous posts at: http://listserv.ipc.org/archives
> > Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> > ext.5315
> > -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2