Werner,
I could use some myself for internal quality training.
I have recently soaked some BGAs and some quad packs in water for over a
week before putting them through a reflow profile. I have yet to produce
visible evidence of pop corning.
The annoying thing is, a while ago we used some BGAs on a tape where the
moisture indicator went just a little pink and they pop corned. The visual
evidence was fat solder deposits and shorts in the middle of the package
where it bowed downwards. My street cred. with the managers around here has
taken a beating since I have failed to reproduce the problem.
Oh well, I'd rather be happy than right.
Regards
Eric Dawson
> -----Original Message-----
> From: Werner Engelmaier [SMTP:[log in to unmask]]
> Sent: Monday, November 18, 2002 4:02 PM
> To: [log in to unmask]
> Subject: [TN] Popcorning
>
> Hi 'Netters,
> Could any of share some good pictures of a 'popcorned' component and a
> component with delaminated die. I would of course give full credit as to
> source.
>
> Thanks,
> Werner Engelmaier
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|