Jim,
we have good experience with Dow Corning Q1-9226. It is a well
established, pasty, 2 component, alumina filled, heat curing (at least
100°C, up to 200°C for snap curing) silicon adhesive with a pot life
(after mixing 1:1 by weight) of about 8 hours. As it is from the
addition curing type, it does not generate byproducts during curing. As
the coherent force (the inner rigidity of the glue) is lower than the
adherent adhesion force, one can increase lap shear forces far above the
values given in the data sheets by making the glue film as thin as
possible (lower than 50 micrometers). This also will give you low
thermal resistivity.
Hope that helped a little
U. Korndörfer (not working for or associated with Dow Corning)
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|