Peter,
Did some work recently on large BNC connectors, the trouble with them is
that the body of the connector acts as a great heat sink thus drawing heat
away from the solder land and connector lead I was trying to solder.
P.s when I contacted the component supplier's they informed me that the
component in question was not suitable for wave solder. We now solder them
with an RF soldering iron.
Hope this is of some use.
Steve.
-----Original Message-----
From: peter lee [mailto:[log in to unmask]]
Sent: 20 November 2001 16:56
To: [log in to unmask]
Subject: [TN] Solder spikes and icicling
Hello,
Can someone explain what are possible causes for wave
soldering spikes and icicling on the assemblies?
I am encountering this defect on boards with larger
BNC connectors and fuse jumpers. Could this be a
pre-heating issue? How would one resolve this?
Rgds,
Peter
__________________________________________________
Do You Yahoo!?
Yahoo! GeoCities - quick and easy web site hosting, just $8.95/month.
http://geocities.yahoo.com/ps/info1
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
_____________________________________________________________________
This message has been checked for all known viruses by Star Internet
delivered through the MessageLabs Virus Scanning Service. For further
information visit http://www.star.net.uk/stats.asp or alternatively call
Star Internet for details on the Virus Scanning Service.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|