TECHNET Archives

March 2018

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Wed, 14 Mar 2018 11:06:53 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (36 lines)
Hi Dave,

Don't know if you have already checked with Berquist Inc. (they deal almost
exclusively with thermal management), but I bet they could help with
selection of a good material or method to heatsink a component.

Steve

On Wed, Mar 14, 2018 at 10:49 AM, Dave Schaefer <[log in to unmask]>
wrote:

> Does anyone have any references to good information regarding the amount
> of compression that can be applied to an SAC BGA component for heat sinking
> purposes? We want to maximize our thermal performance without sacrificing
> solder joint & component reliability.
>



-- 
Steve Gregory
Kimco Design and Manufacturing
Process Engineer
(208) 322-0500 Ext. -3133

-- 


This email and any attachments are only for use by the intended 
recipient(s) and may contain legally privileged, confidential, proprietary 
or otherwise private information. Any unauthorized use, reproduction, 
dissemination, distribution or other disclosure of the contents of this 
e-mail or its attachments is strictly prohibited. If you have received this 
email in error, please notify the sender immediately and delete the 
original. 

ATOM RSS1 RSS2