Hi Dave, Don't know if you have already checked with Berquist Inc. (they deal almost exclusively with thermal management), but I bet they could help with selection of a good material or method to heatsink a component. Steve On Wed, Mar 14, 2018 at 10:49 AM, Dave Schaefer <[log in to unmask]> wrote: > Does anyone have any references to good information regarding the amount > of compression that can be applied to an SAC BGA component for heat sinking > purposes? We want to maximize our thermal performance without sacrificing > solder joint & component reliability. > -- Steve Gregory Kimco Design and Manufacturing Process Engineer (208) 322-0500 Ext. -3133 -- This email and any attachments are only for use by the intended recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original.