TECHNET Archives

September 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
TechNet Mail Forum<[log in to unmask]>
Subject:
From:
Date:
Thu, 4 Sep 1997 08:35:50 PDT
Content-type:
text/plain; charset=US-ASCII
MIME-Version:
1.0
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (19 lines)
Technetters,

        We are investigating the use of a Highly Accelerated Stress Test
(HAST) on a PCB assembly using SMT on standard FR4 with Flex attached to
represent a 20 year storage condition.  The proposed environmental conditions
are 120 C at 98 %RH, unbiased.

        Has anyone performed this type of test and would be willing to comment
on its effectiveness?  We want to minimize test time, develop an acceleration
model to the storage environment, and not introduce new failure modes from the
test itself.

Thanks for any input.

Glenn Pelkey
Quality/Reliability Engineer
Maxtek Components Corp.