Hope this helps. We have an SMT process where some connectors are
given a bead of epoxy along the solder joint to give it additional mechanical
strength. The part then goes through an injection molding process. Tests
have shown the epoxy adds considerable strength to the joint.
Let me know if you need more info, and I'll supply what I can.
Glenn Pelkey
Quality/Reliability Engineer
Maxtek Components Corp.
Sheila Smith <[log in to unmask]> Wrote:
|
| Hi! Does anyone have any experience with using epoxy to
| encapsulate
| components, including the leads, soldered in PTHs? The
| entire assembly is
| subsequently potted with a thermally conductive silicone.
| The goal is to
| keep the solder joint from moving during temperature
| cycling. Any
| suggestions would be appreciated! Thanks, Sheila Smith @
| Tracor AES
|
| ##########################################################
| ####
| TechNet Mail List provided as a free service by IPC using
| LISTSERV 1.8c
| ##########################################################
| ####
| To subscribe/unsubscribe, send a message to
| [log in to unmask] with following text in the body:
| To subscribe: SUBSCRIBE TECHNET <your full name>
| To unsubscribe: SIGNOFF TECHNET
| ##########################################################
| ####
| Please visit IPC web site
| (http://www.ipc.org/html/forum.htm) for additional
| information.
| For the technical support contact Dmitriy Sklyar at
| [log in to unmask] or 847-509-9700 ext.311
| ##########################################################
| ####
|
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|