Hi Charles,
I once faced with the problem on such issue. I solved by using a rubber
squeegee. And I was consistently getting 99.7% yield rate or even higher,
without solder short and unsoldered joint.
I guess many people do not use rubber squeegee nowsaday. Getting a good
print definition is important and getting a good stencil is important so as
to have a good paste release.
And one more important area is the solderpaste. Good paste provides good
print defintion as well as resolving bridging issue.
Sometimes, I use manual printing process on 20 mil pitch components, and so
far there is no issue on bridging and no solder or insufficient solder.
Good Luck.
Poh
At 05:56 PM 2/17/04 -0600, you wrote:
>We have a new assy. that uses 1206 capacitor networks. We are have a serious
>problem with bridging and unsoldered connections. We think we may have solved
>the non soldered problem by increasing the soak before reflow but still have
>the bridging. Anybody have similar experiences? We are using a 5 mil.
>stencil. The other parts all seem to solder well. We are considering having
>the apertures for these parts reduced. Any suggestions would be greatly
>appreciated.
>
>Charles Caswell
>The Big Kahuna
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
>-----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|