Depends upon the alloy and the environment, Werner. I have heard that some
seem to do well at only 20-25 degrees higher, and even better if they are
used in a nitrogen-rich atmosphere (the fillets turn out somewhat shinier,
too). But, the reflow temperatures will indeed be higher with Pb-free
solders. No doubt about it!
Dale Ritzen, CQA
Quality Manager
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Werner Engelmaier
Sent: Wednesday, February 18, 2004 8:22 AM
To: [log in to unmask]
Subject: Re: [TN] Is removal of lead from electronics solders a
legitimate effort?
Hi Ramon,
You are too optimistic--"Not to mention the extra stress that is going to be
placed on the components as the reflow profiles have to be 20 degrees higher
than they are
now"--try mmore like 30 to 35°C.
Werner Engelmaier
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|