The 0.3 % addresses the limit relative to the defect(s) opportunities per
board, check out paragraph 9.1.2 instructions.
































































































-----Original Message-----
From:   TechNet [mailto:[log in to unmask]]
Sent:   Friday, September 18, 1998 1:16 PM
To:     [log in to unmask]; [log in to unmask]
Subject:        [TN] : Corrective Action Limits

 << File: Part.001 >> Replay of message sent Sept. 14th. Does anyone have
anything to say about
this ?

In J-STD-001A, paragraph 9.1.1 speaks to Corrective action limits.

A couple of questions,

1) It states  that corrective action must be initaiated if the Defects
listed in table 11-1 exceed 0.3%.

     - Is that per board, per lot, per day or what ?

2) Corrective action...

     - Is this a form that is filled out ? or is it your own internal system
?
     - What exactly needs to be spelled out  ?

Thanks to all you can spare a sentence or two on this topic.
(I'm just trying to see what others are doing to comply fully to J-STD-001A)

Bill Kasprzak
Moog Inc.

################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2