The 0.3 % addresses the limit relative to the defect(s) opportunities per
board, check out paragraph 9.1.2 instructions.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]
Sent: Friday, September 18, 1998 1:16 PM
To: [log in to unmask]; [log in to unmask]
Subject: [TN] : Corrective Action Limits
<< File: Part.001 >> Replay of message sent Sept. 14th. Does anyone have
anything to say about
this ?
In J-STD-001A, paragraph 9.1.1 speaks to Corrective action limits.
A couple of questions,
1) It states that corrective action must be initaiated if the Defects
listed in table 11-1 exceed 0.3%.
- Is that per board, per lot, per day or what ?
2) Corrective action...
- Is this a form that is filled out ? or is it your own internal system
?
- What exactly needs to be spelled out ?
Thanks to all you can spare a sentence or two on this topic.
(I'm just trying to see what others are doing to comply fully to J-STD-001A)
Bill Kasprzak
Moog Inc.
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|