TECHNET Archives

September 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Rick Thompson <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 22 Sep 2000 13:57:45 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (88 lines)
Steve,

Thanks for the information. Not being too familiar with these things, is
there any problem with pressure sensitive adhesive sticking to parts or am I
looking at a non-issue?  I ask because on occasion we seem to get parts that
randomly stick to the cover tape.

Rick Thompson

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Stephen R. Gregory
Sent: Friday, September 22, 2000 11:16 AM
To: [log in to unmask]
Subject: Re: [TN] Component Taping Equipment?


In a message dated 09/22/2000 12:20:07 PM Central Daylight Time,
[log in to unmask] writes:

> As a small contract manufacturer, we receive alot of components that
aren't
>  machine placeable from our customers.  I'm looking into the possibility
of
>  putting the components on tape and reel in-house.  Any feedback on
vendors
>  for this equipment and the feasability/cost effectiveness of doing this
>  would be appreciated.  Should I even consider it or just send parts out?
>
>  Thanks in advance,
>
>
>  Rick Thompson
>  Ventura Electronics Assembly
>  2665A Park Center Dr.
>  Simi Valley, CA 93065
>
>  +1 (805) 584-9858 voice
>  +1 (805) 584-1529 fax
>  [log in to unmask]

Hi Rick!

We've got a V-Tek machine here...it's a model that I don't think they make
any more...it's called a Compak. It's manual but we don't do any high-volume
tape and reeling. I like it because the set-up is so easy. Uses PSA
(pressure
sensitive adhesive) cover tape, so you don't have to worry about heat shoe
settings or things of that sort...

Go to:

http://www.vtekusa.com/products.htm

There will be their latest models there...they're not that expensive either.
Like I said we don't do any high volume taping, so it fits our needs pretty
good.

-Steve Gregory-

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2