TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
- Bogert <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, - Bogert <[log in to unmask]>
Date:
Mon, 6 Nov 2006 18:13:34 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (134 lines)
November 6, 2006

If you do not clean after soldering using any type of flux, including the no-clean, how do you know there may not be some other form of contamination  present that is unrelated to the flux use; for example residue from the PWB processing, handling of the PWA, residue from component leads, etc.  Is it not possible these could cause equipment operating problems, etc.  Also, what is the problem cleaning PWAs that have no-clean flux? Are you saying that cleaning a no-clean flux will activate what may have been a benign flux?  If so, is there test data available that suupports this?
  ----- Original Message ----- 
  From: Douglas O. Pauls<mailto:[log in to unmask]> 
  To: [log in to unmask]<mailto:[log in to unmask]> 
  Sent: Monday, November 06, 2006 11:26 AM
  Subject: Re: [TN] Cleaning media for no clean paste


  I would agree with Steve.  The Aquanox line has served us well at Rockwell
  and we are converting over to the Kyzen Aquanox A4520 and are getting
  excellent resuls.  I am a proponent of aqueous cleaning since you get both
  the dynamic action of pressurized spray, the thermal activity of hot wash
  and rinse waters, and the chemical energy of a saponifier.  For these
  reasons, I would strongly recommend you stay away from any kind of vapor
  degreasing and no-clean residues.  Bad Karma.

  I guess the more important question is why are you cleaning the low solids
  flux residues and is the low residue paste designed to be cleanable?  Very
  important questions.

  Doug Pauls
  Rockwell Collins




               Steve Gregory
               <SGregory@OAIELEC<mailto:SGregory@OAIELEC>
               TRONICS.COM>                                               To
               Sent by: TechNet          [log in to unmask]<mailto:[log in to unmask]>
               <[log in to unmask]<mailto:[log in to unmask]>>                                          cc

                                                                     Subject
               11/06/2006 10:05          Re: [TN] Cleaning media for no
               AM                        clean paste


               Please respond to
                TechNet E-Mail
                     Forum
               <[log in to unmask]<mailto:[log in to unmask]>>
               ; Please respond
                      to
                 Steve Gregory
               <SGregory@OAIELEC<mailto:SGregory@OAIELEC>
                 TRONICS.COM>






  Hi Dan!

  I've always had very good results cleaning no-clean residues with Kyzen
  Aquanox 4512P in a batch cleaner. They have another formula for
  lead-free residues, Aquanox 4630. They also have another formula
  (Aquanox 4520) that I've not had a chance to use, that is supposed to be
  better than the 4512P. You might want to give them a call...

  -Steve Gregory-

  -----Original Message-----
  From: TechNet [mailto:[log in to unmask]] On Behalf Of Dan Mauro
  Sent: Monday, November 06, 2006 9:56 AM
  To: [log in to unmask]<mailto:[log in to unmask]>
  Subject: [TN] Cleaning media for no clean paste

  Folks,



  I need to clean the residual residue left if any on boards processed
  with no clean paste.

  What should one use.  Any thoughts - is there a common chemical cleaner
  that can penetrate under components.



  Thanks in Advance

  Dan


  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
  unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
  (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET
  Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
  posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest Search the
  archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives> Please
  visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for
  additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or
  847-615-7100 ext.2815
  -----------------------------------------------------

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to
  [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>
  for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or
  847-615-7100 ext.2815
  -----------------------------------------------------

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
  -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2