TECHNET Archives

March 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jenny Drake <[log in to unmask]>
Date:
Mon, 31 Mar 2008 08:04:12 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Creswick, Steven" <[log in to unmask]>
Subject:
From:
"Creswick, Steven" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (36 lines)
Jenny,

I am looking for a distributor in the US.  Were there any leads over
here?

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jenny Drake
Sent: Monday, March 31, 2008 4:20 AM
To: [log in to unmask]
Subject: Re: [TN] Polymer cored solder spheres.

Hi Werner,
    I received a couple of responses off the list and will be chasing
them up. Thanks for the extra suggestions. It was your paper in Global
SMT and Packaging that alerted me to the existence of these balls. Early
days yet and I can't go in to details at this stage, but they might help
in the assembly of our product. All depends on cost and availability. 
 
Best regards,  Jenny

 
 
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer. [gntx v.1]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2