TECHNET Archives

December 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Mon, 21 Dec 1998 18:38:27 +0100
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Matthias Mansfeld <[log in to unmask]>
Content-transfer-encoding:
7BIT
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Matthias Mansfeld <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Organization:
Matthias Mansfeld Elektronik
Comments:
Authenticated sender is <[log in to unmask]>
Parts/Attachments:
text/plain (32 lines)
On 21 Dec 98 at 7:29, Mike Bailey wrote:

> We continue to see current designs incorporating via hole
> configurations utilizing "wagon wheel" interconnects to plane
> layers.
I use direct connects whenever no thermal reasons need "wagon wheel"
style. That means, vias (no THT holes) without thermals,
and all thru-holes with leaded components which become hand- or
wave-soldered, with thermals. I can set up this without problems in
my CAD system which type of hole gets spokes or not by default.
Regards
Matthias
-----------------------------------------------
Matthias Mansfeld Elektronik
* Printed Circuit Board Design and Assembly
Am Langhoelzl 11, D-85540 Haar, GERMANY
Phone: +49-89-4620 0937, Fax: +49-89-4620 0938
E-Mail: [log in to unmask]
Internet: http://www.mansfeld-elektronik.de

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2