Hi, netters!
As a producer of CCL, we routinely check dielectric
constant (Dk) of our laminates at 1 Mhz
Recently, some customers want Dk at Ghz range, which we can
not measure.
Does anybody know reliable Dk testing service for laminates
at Ghz range?
We have HP instrument which has the capability of measuring
Dk up to 10 Ghz.
However, we just do not know how to measure Dk of our
products, laminates.
We heard that a specially designed fixture is needed for
the laminate.
Did anyone measure Dk of PCB laminate at Ghz ?
What kinds of fixture did you use?
Or is there any hands-on training course about Dk
measurements?
Minsu Lee
Doosan Electro-materials Co.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|