TECHNET Archives

June 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Douglas Pauls <[log in to unmask]>
Date:
Wed, 1 Jun 2016 16:33:22 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Mike Fenner <[log in to unmask]>
Message-ID:
<1BAA34A8776B4A45AB2CC518A67D93C4@MikePC>
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (40 lines)
So what are ionising fans - as sold by static control companies then?


-- 
Regards 
 
Mike 
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Wednesday, June 01, 2016 3:14 PM
To: [log in to unmask]
Subject: [TN] Fans and ESD

Good morning all,

We had an outside audit "observation" that I would like some outside
opinions on.  In your facilities, are simple air circulation fans, usually
plastic blades and a plastic housing (think inexpensive Walmart) targeted
as an ESD generator?  I have never heard of such and my view is that if our
humidity stays above the 30% minimum found in most ESD standards, then we
should not have charge generation.

So, are cheapy plastic fans an ESD hazard?

Doug Pauls
Principal Materials and Process Engineer
Rockwell Collins


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2