Hey, I was just trying to keep it anonymous so my friends in the solder
paste biz do not worry to much. Thanks for being so detailed and thorough.
.......wise guy's ;-)
Just to emphasize again. The flux is being removed 100%. Verified by
removing a part right after the wash and rinsing w/IPA. The solder joints
look ok no residue!
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Wednesday, May 01, 2002 3:11 PM
To: [log in to unmask]
Subject: Re: [TN] High lead composition solder paste and rinse water.
George points out:
95Pb/5Sn/2.5Ag adds up to 102.5%
Doug points out:
102.5% can lead to excessive solder joints, or the flux manufacturers have
found a way to manufacture a -2.5% solids flux........
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----