TECHNET Archives

November 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Franklin D Asbell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Date:
Mon, 15 Nov 2004 15:08:51 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (23 lines)
I'm thinking it's not so much a solder mask issue as a cleanliness issue
before the application of solder mask.

Dendritic growth is probably what is occurring. Contaminates on the
copper/glass prior to solder mask are occurring with the application of
current, causing these growths to bridge traces causing shorts.

A good precleaning process, pumice scrub followed by chemical clean perhaps,
would remove all contaminates that may cause these growths, and subsequent
shorts.

Franklin

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2