HIP - HOP it's all the same to me......8-)
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*
Sent: Friday, July 17, 2009 9:19 AM
To: [log in to unmask]
Subject: Re: [TN] [SMART] Head In Pillow Joints->Head On Pillow
'Head In Pillow' sure is a strange terminology--'Head On Pilow' is by far
more descriptive
Werner
-----Original Message-----
From: Mike Fenner <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, Jul 17, 2009 5:03 am
Subject: Re: [TN] [SMART] Head In Pillow Joints
Since 2001? Ingenious as ever John, but perhaps it maybe time to look at
more modern materials which address this issue without mechanical aids.
Regards
Mike
_____
From: SMART Group smart-e-link [mailto:[log in to unmask]] On
Behalf Of John Burke
Sent: 16 July 2009 18:51
To: [log in to unmask]
Subject: Re: [SMART] Head In Pillow Joints
Quite often seen as a field failure since due to the compression of the head
in pillow interface it is quite possible to test and get signals through
only to find it fails in the field.
Data for this defect would be best found from companies using large BGA's
say above 20 x 20 mm with smaller BGA pitch - say 0.8mm and below, and
taking both their internal records of such failures and mapping it with RMA
returns for the same defect. Truth is, this defect actually in many cases
results in an RMA return where upon return there is NTF (No trouble found).
If you really want to find if you have this condition in your manufacturing
process the only way to completely engineer it out is to include a vibration
under power and use test during the pilot runs to tune in the reflo
w
profile.
I have used this method since 2001.
John
John Burke
(408) 515 4992
_____
From: SMART Group smart-e-link [mailto:[log in to unmask]] On
Behalf Of bob Willis
Sent: Thursday, July 16, 2009 9:25 AM
To: [log in to unmask]
Subject: Re: [SMART] Head In Pillow Joints
_____
<http://www.smartgroup.org> SMART logo
smart-e-link is an e-mail technical forum organised by the SMART Group.
Visit our webpage <http://www.smartgroup.org/smtlink.htm> for subscription
information, rules of use and any questions.
smart-e-link is sponsored by Soldertec Global <http://www.soldertec.com> -
a business providing laboratory testing, troubleshooting, and analytical
services to the global electronics industry. Services include x-ray
inspection, scanning electron microscopy, solderability testing, SIR and in
testing of components and materials for compliance with the RoHS Directive.
Visit www.soldertec.com.
To unsubscribe to smart-e-link, send an e-mail to
[log in to unmask] with the following text in the body (not the
subject field): SIGNOFF smart-e-link.
<http://lists.smartgroup.org/archives/smart-e-link.html> smart-e-link is
archived on the web.
_____
<http://www.smartgroup.org> SMART logo smart-e-link is an e-mail technical
forum organised by the SMART Group. Visit our webpage
<http://www.smartgroup.org/smtlink.htm> for subscription information, rules
of use and any questions.
smart-e-link is sponsored by Soldertec Global <http://www.soldertec.com> -
a business
providing laboratory testing, troubleshooting, and analytical
services to the global electronics industry. Services include x-ray
inspection, scanning electron microscopy, solderability testing, SIR and in
testing of components and materials for compliance with the RoHS Directive.
Visit www.soldertec.com.
To unsubscribe to smart-e-link, send an e-mail to
[log in to unmask] with the following text in the body (not the
subject field): SIGNOFF smart-e-link.
<http://lists.smartgroup.org/archives/smart-e-link.html> smart-e-link is
archived on the web.
***This email, its content, and any files transmitted with it, are intended
solely for the addressee(s) and may be legally privileged and/or
confidential.
If you are not the intended recipient, please contact the sender by return
and
delete the material from any computer. Any review, retransmission,
dissemination, or other use of, or taking of any action in reliance upon
this
information by persons or entities other than the intended recipient is
prohibited.
Messages sent via this medium may be subjected to delays, non-delivery, and
unauthorized alteration. This email has been prepared using information
believed
by the author to be reliable and accurate, but Indium Corporation makes no
warranty as to accuracy or completeness. Indium Corporation does not accept
responsibility for changes made to this email after is was sent. Any
opinions or
recommendations expressed herein are solely those of the author. They may be
subject to change without notice.***
---------------
------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|