TECHNET Archives

December 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Terry L. Munson" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 11 Dec 2009 17:11:09 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (113 lines)
Dave
I would agree that ROSA would be effective for only a couple hours.   We 
have been very effective at removing oxides with plasma and even to the point  
of stripping paralyene coating that is 4-5 mil.  
 
 
In a message dated 12/11/2009 8:11:19 A.M. Eastern Standard Time,  
[log in to unmask] writes:

Hi Guy!  Yes the ROSA (Reduced Oxide Soldering Activation) process would be 
able to  restore a HASL surface finish but I probably have the only 
remaining  functioning system in the industry. Secondly, you need to 
process the  "restored" pwb within a few hours after ROSA treatment or the  
effectiveness is lost . I could restore Lee's pwb solderability but I  
couldn't get it shipped to him in time before it would it would  
re-oxidized. As several other TechNet contributors have suggested, a very  
controlled re-HASL process with the correct flux and cleaning processes  
could be a potential option.

Dave



Guy Ramsey  <[log in to unmask]> 
Sent by: TechNet  <[log in to unmask]>
12/10/2009 06:55 PM
Please respond to
TechNet  E-Mail Forum <[log in to unmask]>; Please respond to
Guy Ramsey  <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re:  [TN] BOARD SOLDERABILITY






Remember that tank we had  at ACI that was did electrochemical reduction. 
It was a Rockwell invention  I think, ROSA? It could restore solderability 
to some metals. I don't know  how it would get through the HASL. 

-----Original Message-----
From:  TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman
Sent: Thursday,  December 10, 2009 1:54 PM
To: [log in to unmask]
Subject: [TN] BOARD  SOLDERABILITY

One of my colleagues has a HASL finished board, that sat  in our stockroom 
for ~ 10 years, and of course he want to use them (EOY  Billing).

Ran the board through wave soldering, and it did not solder  at all. Good 
news was that the board was not damaged by the heat - it just  was not 
solderable. I do not want to use a more active flux since it will  be 
difficult to clean.

Are there any solutions / processes that can  restore board solderability?

Thanks in advance.

Lee Whiteman,  PMP
Senior Member Engineering Staff
L-3 Communications  East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail:  [log in to unmask]

---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe,  send a message to [log in to unmask] with following text in
the BODY (NOT the  subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery  of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or  (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to  
[log in to unmask]: SET Technet Digest
Search the archives of previous  posts at: http://listserv.ipc.org/archives
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional  information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100  ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe,  send a message to [log in to unmask] with following text in
the BODY (NOT the  subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery  of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To  receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]:  SET Technet Digest
Search the archives of previous posts at:  http://listserv.ipc.org/archives
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information,  or contact Keach Sasamori at [log in to unmask] or 
847-615-7100  ext.2815
-----------------------------------------------------



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2