TECHNET Archives

May 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 19 May 2000 17:06:32 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
"Stephen R. Gregory" <[log in to unmask]>
Parts/Attachments:
text/plain (40 lines)
In a message dated 05/19/2000 3:50:51 PM Central Daylight Time,
[log in to unmask] writes:

<< I hope those parts aren't soldered into a pcb already!!!

  Roger M. Stoops,       PCB Designer

  Spectra Precision Inc. Ph:     937.233.8921
  5475 Kellenburger Rd.     937.233.4574 ext
  Dayton, OH 45424-1099  288
  USA                    Fax:    937.233.7511  >>

Thanks Roger!

Well they were, but only on 5-boards...we were about to build 150-boards but
the line got stopped for other reasons. The 5-boards got to test and that's
when we found out about the problem...so we were lucky that we only built the
5...unlucky that all the parts for the work order have the bad program...

There are two waferscale devices on the board, one is $18.00 each, the other
is $15.00 a pop...

Glad I'm not a test guy...

-Steve Gregory-

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2